Hi Josh

Our team had a question on the recommendation part of the report.
So after recommendation, are we supposed to include a new true stress and true strain curve?
or do we keep the true stress and strain curve that we obtained during the lab, even after our recommendation?


Thank you
Back to top Go down
View user profile
GSI Overlord
Admin


Posts : 126
Join date : 2012-08-30

PostSubject: Re: Question about what we need to do for recommendation   Sun Sep 30, 2012 5:44 pm

You just need to report the yield stress of your final product (processed brass) with uncertainty, and that needs to be consistent with your nominal stress-strain curve. You could re-plot the nominal stress-strain curve with and show where the final product will lie on that curve, or maybe just put an X (with error bars!) on the curve to signify the final yield stress of the finished product.

Also, I'm not quite sure what you mean by a 'new' true stress and true strain curve...there's only one for the given brass material.

I think as a procedural point you aren't supposed to be including figures in your recommendations, but you could check with the Tech Com people about that.
Back to top Go down
View user profile http://fall2012me395.forumstopic.com
 
Question about what we need to do for recommendation
Back to top 
Page 1 of 1

Permissions in this forum:You cannot reply to topics in this forum
Fall 2012 ME 395 - GSI Josh Lacey :: Lab Questions :: Lab 3-
Jump to: